Facile synthesis of KaCs1−aPbBr3@ molecular sieve SBA-15 composite with improved luminescence and wet/thermal stability 期刊论文
Colloids and Surfaces A: Physicochemical and Engineering Aspects, 2022, 卷号: 648
作者:  Dong, Qizheng;  Tian, Binglong;  Zhang, Wenbo;  He, Ling
收藏  |  浏览/下载:36/0  |  提交时间:2022/06/20
Structure, photoluminescence and abnormal thermal quenching behavior of Eu2+-doped Na3Sc2(PO4)3: A novel blue-emitting phosphor for n-UV LEDs 期刊论文
Journal of Materials Chemistry C, 2016, 卷号: 4, 期号: 37, 页码: 8795-8801
作者:  Wang, Xicheng;  Zhao, Zhengyan;  Wu, Quansheng;  Wang, Chuang;  Wang, Qian
收藏  |  浏览/下载:3/0  |  提交时间:2017/01/13
Effect of lithium ion doping on cubic gd1.88eu0.12o3: enhancement of photoluminescence and thermal stability 期刊论文
Journal of luminescence, 2015, 卷号: 166, 页码: 238-243
作者:  Kang, Yipu;  Shimokawa, Yohei;  Ishihara, Yasutaka;  Miao, Lei;  Tanemura, Sakae
收藏  |  浏览/下载:34/0  |  提交时间:2019/05/09
Effect of lithium ion doping on cubic Gd1.88Eu0.12O3: Enhancement of photoluminescence and thermal stability 期刊论文
journal of luminescence, 2015, 卷号: 166, 页码: 238-243
作者:  Kang, Yipu;  Shimokawa, Yohei;  Ishihara, Yasutaka;  Miao, Lei;  Tanemura, Sakae
收藏  |  浏览/下载:21/0  |  提交时间:2016/12/01
Effect of thickness on the structural, electrical and optical properties of ZnO films deposited by MBE (EI CONFERENCE) 会议论文
2011 International Conference on Advanced Design and Manufacturing Engineering, ADME 2011, September 16, 2011 - September 18, 2011, Guangzhou, China
Yang X.; Su S.; Yi X.; Mei T.
收藏  |  浏览/下载:22/0  |  提交时间:2013/03/25
A set of ZnO films of different thickness have been deposited on sapphire substrates using molecular beam epitaxy (MBE) by varying the growth time and the effect of film thickness on the structural  electrical and optical properties have been investigated. The X-ray diffraction (XRD) results indicate that the full width at half maximum (FWHM) of the (002) diffraction peak is decreased as the film thickness increasing  and the stress along c-axis is stable. Scanning electron microscope (SEM) measurement shows that the grains become more uniform as the film grows thicker and the film surface present distinct hexagon shape as the film is grown up to a thickness of 500nm. The optical absorbance  Hall mobility and photoluminescence (PL) intensity are increased in accordance with the thickness of the film. (2011) Trans Tech Publications  Switzerland.  
Study of photoluminescences of the Ar+implanted porous silicon and the porous structure of Ar+-implanted silicon 期刊论文
Guangdianzi Jiguang/Journal of Optoelectronics Laser, 2008, 卷号: 19, 期号: 12, 页码: 1640-1643
作者:  Lv, Xiao-Yi;  Yang, Yong-Bing;  Jia, Zhen-Hong;  Xue, Tao
收藏  |  浏览/下载:1/0  |  提交时间:2019/12/18
The study of optical property for CdS nanocrystalline prepared by precipitation method (EI CONFERENCE) 会议论文
ICO20: Materials and Nanostructures, August 21, 2005 - August 26, 2005, Changchun, China
Fu Z.; Zhou S.; Li W.; Zhang S.
收藏  |  浏览/下载:16/0  |  提交时间:2013/03/25
Optical characterization of bare CdSe and CdSe/CdS core/shell nanocrystals (EI CONFERENCE) 会议论文
ICO20: Biomedical Optics, August 21, 2005 - August 26, 2005, Changchun, China
An L. M.; Sun P. N.; Liu L.; Feng X.; Kong L. P.; Bi H. N.; Yu B.; Kong X. G.; Liu Y. C.
收藏  |  浏览/下载:12/0  |  提交时间:2013/03/25
Thiol-capped CdSe/CdS core/shell nanocrystals (NCs) which show high luminescence quantum yield are synthesized in an aqueous solution. UV-Vis absorption spectroscopy and photoluminescence (PL) spectroscopy are employed to analyze optical characters and stabilities of NCs. Furthermore  PL properties are studied in a temperature range between 77K and 300K. The PL peak position of bare CdSe NCs shifts toward shorter wavelengths and the band becomes sharper with decreasing temperature. On the same condition  the PL peak position of CdSe/CdS core/shell NCs keeps unconverted nearly with the variation of temperature. Photostability of bare CdSe NCs and CdSe/CdS core/shell NCs are compared under the 325nm laser irradiation. It takes 78 seconds that the PL intensity declines to the half for CdSe NCs  but 442 seconds for CdSe/CdS core/shell NCs. The fluorescence decay lifetime increases about six times after overcoating. The results indicate that the CdS shell can improve the low temperature PL stability and photostability of CdSe NCs effectively.  