已选(0)清除
条数/页: 排序方式:
|
| Influence of Indenter Tip Roundness on Hardness Behavior in Nanoindentation 期刊论文 Materials Science and Engineering A-Structural Materials Properties Microstructure and Processing, 2007, 卷号: 445, 页码: 323-327 作者: Chen WM(陈伟民); Li M(李敏); Zhang TH(张泰华) 收藏  |  浏览/下载:1653/55  |  提交时间:2007/06/15 |
| A New Modified Expanding Cavity Model for Characterizing the Spherical Indentation Behaviour of Bulk Metallic Glass with Pile-up 期刊论文 Scripta Materialia, 2007, 卷号: 56, 期号: 9, 页码: 761-764 作者: Ai K(艾科); Dai LH(戴兰宏) 收藏  |  浏览/下载:1203/151  |  提交时间:2007/06/15 |
| Strain Rate Dependence of Plastic Flow in Ce-based Bulk Metallic Glass During Nanoindentation 期刊论文 Journal of Materials Research, 2007, 卷号: 22, 期号: 2, 页码: 258-263 作者: Wei BC(魏炳忱); Zhang LC(张凌晨); Zhang TH(张泰华) 收藏  |  浏览/下载:1610/91  |  提交时间:2007/06/15 |
| Nonlinear Analysis of Oscillatory Indentation in Elastic and Viscoelastic Solids 期刊论文 Physical Review Letters, 2006, 卷号: 97, 期号: 7, 页码: 075506 作者: Cheng YT; Ni WY; Zheng ZM(郑哲敏) 收藏  |  浏览/下载:1354/152  |  提交时间:2007/06/15 |
| MD Simulation of Phase Transformations Due to Nanoscale Cutting on Silicon Monocrystals with Diamond Tip 期刊论文 Journal of Physics D-Applied Physics, 2006, 卷号: 39, 期号: 16, 页码: 3674-3679 作者: Tang QH(汤奇恒); Chen FH(陈风华) 收藏  |  浏览/下载:2077/228  |  提交时间:2007/06/15 |
| Evaluation of the Effectiveness of Representative Methods for Determining Young's Modulus and Hardness from Instrumented Indentation Data 期刊论文 Journal of Materials Research, 2006, 卷号: 21, 期号: 1, 页码: 225-233 作者: Ma DJ; Zhang TH(张泰华); Ong CW 收藏  |  浏览/下载:1970/191  |  提交时间:2007/06/15 |
| Instrumented Indentation Study of Plastic Deformation in Bulk Metallic Glasses 期刊论文 Journal of Materials Research, 2006, 卷号: 21, 期号: 1, 页码: 75-81 作者: Li WH(李维火); Zhang TH(张泰华); Xing DM(邢冬梅); Wei BC(魏炳忱); Zhang LC(张凌晨) 收藏  |  浏览/下载:1659/115  |  提交时间:2007/06/15 |
| Nonuniformity Effect of Surface-Nanocrystalline Materials in Nanoindentation Test 期刊论文 International Journal for Multiscale Computational Engineering, 2006, 卷号: 4, 期号: 1, 页码: 183-196 作者: Wei YG(魏悦广); Chen XL(陈小亮); Shu SQ(舒思齐) 收藏  |  浏览/下载:1788/66  |  提交时间:2007/06/15 |
| Effect of structural relaxation on deformation behaviour of Zr-based metallic glass 期刊论文 Chinese Physics Letters, 2006, 卷号: 23, 期号: 7, 页码: 1868-1871 作者: Liu Y(刘渊); Zhang TH(张泰华); Wei BC(魏炳忱); Xing DM(邢冬梅); Li WH(李维火) 收藏  |  浏览/下载:778/61  |  提交时间:2007/06/15 |
| Deformation Behavior During Nanoindentation in Ce-Based Bulk Metallic Glasses 期刊论文 Chinese Science Bulletin/中国科学通报(英文版), 2006, 卷号: 51, 期号: 13, 页码: 1639-1643 作者: Zhang LC(张凌晨); Xing DM(邢冬梅); Wei BC(魏炳忱); Wei BC(魏炳忱); Li WH(李维火) 收藏  |  浏览/下载:2102/247  |  提交时间:2007/06/15 |