Preparation of Ti-enriched slag from V-bearing titanomagnetite by two-stage hydrochloric acid leaching route
Zhong, Binnian1,2; Xue, Tianyan1; Zhao, Longsheng1; Zhao, Hongxin1; Qi, Tao1; Chen, Weiliang2
刊名SEPARATION AND PURIFICATION TECHNOLOGY
2014-11-24
卷号137期号:NOV.页码:59-65
关键词V-Ti concentrate Hydrochloric acid leaching Molecular simulation Impurity separation Ti-enriched slag
ISSN号1383-5866
其他题名Sep. Purif. Technol.
中文摘要Low-grade, highly reactive V-Ti concentrate was obtained from V-bearing titanomagnetite via selective reduction-magnetic separation. The main phases of the concentrate are anosovite and pyroxene. Two-stage acid leaching was employed to remove the impurities in the concentrate. The leaching behavior of impurities Ca/Mg/Al/Si under different acid leaching conditions in the first stage was investigated in detail. The optimal leaching conditions of the first-stage were as follows: 383 K leaching temperature, 1.40 mol/L HCl concentration, 1/10 solid-liquid mass ratio, and 120 min leaching time, under which the residue obtained contained 79.54% of TiO2 and 2.50% of V2O5. The result of molecular structure simulation indicate that the Ti-O and Mg-O bonds in the anosovite phase are broken under oxygen pressure conditions in the second stage by reacted with HCl solution. The content of TiO2 in the Ti-enriched slag prepared by two-stage acid leaching can reach 92.5% with further removal of residual carbon. (C) 2014 Elsevier B.V. All rights reserved.
英文摘要Low-grade, highly reactive V-Ti concentrate was obtained from V-bearing titanomagnetite via selective reduction-magnetic separation. The main phases of the concentrate are anosovite and pyroxene. Two-stage acid leaching was employed to remove the impurities in the concentrate. The leaching behavior of impurities Ca/Mg/Al/Si under different acid leaching conditions in the first stage was investigated in detail. The optimal leaching conditions of the first-stage were as follows: 383 K leaching temperature, 1.40 mol/L HCl concentration, 1/10 solid-liquid mass ratio, and 120 min leaching time, under which the residue obtained contained 79.54% of TiO2 and 2.50% of V2O5. The result of molecular structure simulation indicate that the Ti-O and Mg-O bonds in the anosovite phase are broken under oxygen pressure conditions in the second stage by reacted with HCl solution. The content of TiO2 in the Ti-enriched slag prepared by two-stage acid leaching can reach 92.5% with further removal of residual carbon. (C) 2014 Elsevier B.V. All rights reserved.
WOS标题词Science & Technology ; Technology
类目[WOS]Engineering, Chemical
研究领域[WOS]Engineering
关键词[WOS]TITANIUM-DIOXIDE ; ILMENITE
收录类别SCI
原文出处://WOS:000345181500008
语种英语
WOS记录号WOS:000345181500008
公开日期2015-04-01
内容类型期刊论文
源URL[http://ir.ipe.ac.cn/handle/122111/11905]  
专题过程工程研究所_研究所(批量导入)
作者单位1.Chinese Acad Sci, Inst Proc Engn, Key Lab Green Proc & Engn, Beijing 100190, Peoples R China
2.Kunming Univ Sci & Technol, Fac Met & Energy Engn, Natl Engn Lab Vacuum Met, Kunming 650093, Peoples R China
推荐引用方式
GB/T 7714
Zhong, Binnian,Xue, Tianyan,Zhao, Longsheng,et al. Preparation of Ti-enriched slag from V-bearing titanomagnetite by two-stage hydrochloric acid leaching route[J]. SEPARATION AND PURIFICATION TECHNOLOGY,2014,137(NOV.):59-65.
APA Zhong, Binnian,Xue, Tianyan,Zhao, Longsheng,Zhao, Hongxin,Qi, Tao,&Chen, Weiliang.(2014).Preparation of Ti-enriched slag from V-bearing titanomagnetite by two-stage hydrochloric acid leaching route.SEPARATION AND PURIFICATION TECHNOLOGY,137(NOV.),59-65.
MLA Zhong, Binnian,et al."Preparation of Ti-enriched slag from V-bearing titanomagnetite by two-stage hydrochloric acid leaching route".SEPARATION AND PURIFICATION TECHNOLOGY 137.NOV.(2014):59-65.
个性服务
查看访问统计
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。


©版权所有 ©2017 CSpace - Powered by CSpace