Effects of CNTs content on microstructure and mechanical properties of Cnt/α-Al2O3 and Cnt-Csf/α-Al2O3 composites | |
Jia, Jiangang1; Liu, Diqiang1,2; Zhang, Sheng1; Zhang, Bo1; Liu, Shunwei1; Ji, Genshun1 | |
刊名 | Ceramics International
![]() |
2019-11-01 | |
卷号 | 45期号:16页码:19956-19961 |
关键词 | Alumina Aluminum oxide Bending strength Hot pressing Sol-gel process Sol-gels Textures Alpha-Al2O3 CNTs Hot-pressing process Matrix composite Microstructure and mechanical properties Relative density Short carbon fibers Transgranular fracture |
ISSN号 | 02728842 |
DOI | 10.1016/j.ceramint.2019.06.253 |
英文摘要 | In this work, CNTs and short carbon fiber reinforced α-Al2O3 matrix composites (i.e., Cnt/α-Al2O3 and Cnt-Csf/α-Al2O3) were prepared by sol-gel dispersing method followed by hot pressing process. Effects of CNTs content on the mechanical properties of Cnt/α-Al2O3 and Cnt-Csf/α-Al2O3 composites were investigated and the inter- and transgranular fracture mechanisms in Cnt-Csf/α-Al2O3 composites were analyzed. The hardness and relative density of Cnt/α-Al2O3 and Cnt-Csf/α-Al2O3 composites slightly decrease as CNTs content increases. The flexural strength and fracture toughness monotonically increase with the increase in Cnt content for both Cnt/α-Al2O3 and Cnt-Csf/α-Al2O3 composites. Addition of Csf and CNTs into α-Al2O3 matrix results in a bimodal grain size microstructure of Cnt-Csf/α-Al2O3 composites, which accounts for the unique fractograph and the enhanced toughness of Cnt-Cf/α-Al2O3 composites. The flexural strength and fracture toughness of Csf5-nt06 composite are 465 MPa and 7.08 MPa/m2, 37% and 13% higher than that of Cnt06, and 42% and 34% higher than that of Csf5, respectively. © 2019 Elsevier Ltd and Techna Group S.r.l. |
WOS研究方向 | Materials Science |
语种 | 英语 |
出版者 | Elsevier Ltd |
WOS记录号 | WOS:000488148100043 |
内容类型 | 期刊论文 |
源URL | [http://ir.lut.edu.cn/handle/2XXMBERH/114362] ![]() |
专题 | 材料科学与工程学院 |
作者单位 | 1.State Key Laboratory of Advanced Processing and Recycling of Non-ferrous Metals, Lanzhou University of Technology, Lanzhou; 730050, China; 2.School of Materials Science and Engineering, North University of China, Taiyuan; 030051, China |
推荐引用方式 GB/T 7714 | Jia, Jiangang,Liu, Diqiang,Zhang, Sheng,et al. Effects of CNTs content on microstructure and mechanical properties of Cnt/α-Al2O3 and Cnt-Csf/α-Al2O3 composites[J]. Ceramics International,2019,45(16):19956-19961. |
APA | Jia, Jiangang,Liu, Diqiang,Zhang, Sheng,Zhang, Bo,Liu, Shunwei,&Ji, Genshun.(2019).Effects of CNTs content on microstructure and mechanical properties of Cnt/α-Al2O3 and Cnt-Csf/α-Al2O3 composites.Ceramics International,45(16),19956-19961. |
MLA | Jia, Jiangang,et al."Effects of CNTs content on microstructure and mechanical properties of Cnt/α-Al2O3 and Cnt-Csf/α-Al2O3 composites".Ceramics International 45.16(2019):19956-19961. |
个性服务 |
查看访问统计 |
相关权益政策 |
暂无数据 |
收藏/分享 |
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。
修改评论