英文摘要 | Cobalt-based and nickel-based coatings were successfully produced using TIG welding and laser cladding technologies as alternative materials with higher cavitation erosion (CE) and slurry erosion (SE) resistance, respectively. Their structure, phase constitution, hardness and elastoplasticity were characterized. Combined with the cumulative mass loss, erosion morphology and roughness, the CE and SE resistances were compared and erosion models were also proposed. The results show that the cobalt-based coating exhibited much better CE resistance and lower SE resistance than the nickel-based coating. The phase transition contributes mostly to the high CE resistance of the cobalt-based coating. While, the combined effects of high hardness, elastoplasticity and hard phases' anchoring and shielding, determine the high SE resistance of the nickel-based coating. |
资助项目 | National Key R&D Program of China[2018YFC0808500] ; National Natural Science Foundation of China[51501206] ; CAS Key Laboratory of Nuclear Materials and safety Assessment[2017NMSAKF03] |
WOS研究方向 | Engineering ; Materials Science |
语种 | 英语 |
出版者 | ELSEVIER SCIENCE SA |
WOS记录号 | WOS:000471596300024 |
资助机构 | National Key R&D Program of China ; National Natural Science Foundation of China ; CAS Key Laboratory of Nuclear Materials and safety Assessment |
内容类型 | 期刊论文 |
源URL | [http://ir.imr.ac.cn/handle/321006/134189] |
专题 | 金属研究所_中国科学院金属研究所 |
通讯作者 | Hu, H. X. |
作者单位 | 1.Chinese Acad Sci, Inst Met Res, CAS Key Lab Nucl Mat & Safety Assessment, Shenyang 110016, Liaoning, Peoples R China 2.Shenyang Aerosp Univ, Sch Mat Sci & Engn, Shenyang 110136, Liaoning, Peoples R China |
推荐引用方式 GB/T 7714 | E, M.,Hu, H. X.,Guo, X. M.,et al. Comparison of the cavitation erosion and slurry erosion behavior of cobalt-based and nickel-based coatings[J]. WEAR,2019,428:246-257. |
APA | E, M.,Hu, H. X.,Guo, X. M.,&Zheng, Y. G..(2019).Comparison of the cavitation erosion and slurry erosion behavior of cobalt-based and nickel-based coatings.WEAR,428,246-257. |
MLA | E, M.,et al."Comparison of the cavitation erosion and slurry erosion behavior of cobalt-based and nickel-based coatings".WEAR 428(2019):246-257. |
个性服务 |
查看访问统计 |
相关权益政策 |
暂无数据 |
收藏/分享 |
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。
修改评论