Failure criterion of buried pipelines with dent and scratch defects | |
Tian, Xiao; Zhang, Hong | |
刊名 | ENGINEERING FAILURE ANALYSIS |
2017 | |
卷号 | 80页码:278-289 |
关键词 | Dent Scratch Tensile strength Finite element analysis Failure criterion |
ISSN号 | 1350-6307 |
DOI | 10.1016/j.engfailanal.2017.06.049 |
URL标识 | 查看原文 |
收录类别 | SCIE ; EI |
WOS记录号 | WOS:000407182600023 |
内容类型 | 期刊论文 |
URI标识 | http://www.corc.org.cn/handle/1471x/6270920 |
专题 | 中国石油大学(北京) |
推荐引用方式 GB/T 7714 | Tian, Xiao,Zhang, Hong. Failure criterion of buried pipelines with dent and scratch defects[J]. ENGINEERING FAILURE ANALYSIS,2017,80:278-289. |
APA | Tian, Xiao,&Zhang, Hong.(2017).Failure criterion of buried pipelines with dent and scratch defects.ENGINEERING FAILURE ANALYSIS,80,278-289. |