Very High Cycle Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy DZ4 | |
Nie, Baohua; Zhao, Zihua; Liu, Shu; Chen, Dongchu; Ouyang, Yongzhong; Hu, Zhudong; Fan, Touwen; Sun, Haibo | |
刊名 | MATERIALS
![]() |
2018 | |
卷号 | 11 |
关键词 | DZ4 casting defects VHCF crack initiation |
ISSN号 | 1996-1944 |
DOI | 10.3390/ma11010098 |
URL标识 | 查看原文 |
收录类别 | SCIE ; EI ; PUBMED |
WOS记录号 | WOS:000427764000098 |
内容类型 | 期刊论文 |
URI标识 | http://www.corc.org.cn/handle/1471x/5935843 |
专题 | 北京航空航天大学 |
推荐引用方式 GB/T 7714 | Nie, Baohua,Zhao, Zihua,Liu, Shu,et al. Very High Cycle Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy DZ4[J]. MATERIALS,2018,11. |
APA | Nie, Baohua.,Zhao, Zihua.,Liu, Shu.,Chen, Dongchu.,Ouyang, Yongzhong.,...&Sun, Haibo.(2018).Very High Cycle Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy DZ4.MATERIALS,11. |
MLA | Nie, Baohua,et al."Very High Cycle Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy DZ4".MATERIALS 11(2018). |
个性服务 |
查看访问统计 |
相关权益政策 |
暂无数据 |
收藏/分享 |
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。
修改评论