Acoustic emission response of 304 stainless steel during constant load test in high temperature aqueous environment | |
J. Xu ; E. H. Han ; X. Q. Wu | |
刊名 | Corrosion Science |
2012 | |
卷号 | 63页码:91-99 |
关键词 | Stainless steel SEM Stress corrosion stress-corrosion cracking oxide-film properties stainless-steels electrochemical-behavior ae response water alloy propagation noise |
ISSN号 | 0010-938X |
中文摘要 | Acoustic emission (AE) behavior of 304 stainless steel during constant load test in high temperature aqueous environment was investigated in situ and the corresponding fracture characteristic was examined carefully. The cumulative hits increase with stress intensity factor and two types of signals can be distinguished. According to the fracture morphology and amplitude distribution exponent analysis, it is believed that the high amplitude signals could be attributed to crack propagation and low amplitude ones are due to plastic deformation. The correlation between AE signal evolution and cracking process is discussed. (C) 2012 Elsevier Ltd. All rights reserved. |
原文出处 | |
公开日期 | 2013-02-05 |
内容类型 | 期刊论文 |
源URL | [http://ir.imr.ac.cn/handle/321006/60365] |
专题 | 金属研究所_中国科学院金属研究所 |
推荐引用方式 GB/T 7714 | J. Xu,E. H. Han,X. Q. Wu. Acoustic emission response of 304 stainless steel during constant load test in high temperature aqueous environment[J]. Corrosion Science,2012,63:91-99. |
APA | J. Xu,E. H. Han,&X. Q. Wu.(2012).Acoustic emission response of 304 stainless steel during constant load test in high temperature aqueous environment.Corrosion Science,63,91-99. |
MLA | J. Xu,et al."Acoustic emission response of 304 stainless steel during constant load test in high temperature aqueous environment".Corrosion Science 63(2012):91-99. |
个性服务 |
查看访问统计 |
相关权益政策 |
暂无数据 |
收藏/分享 |
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。
修改评论