Effect of mesoporous silica molecular sieve coating on nZVI for 2,4-DCP degradation: Morphology and mechanism during the reaction.
Wan, Junjie; Feng, Xin; Li, Yu; He, Jinqiang; Zhao, Na; Liu, Zhifeng; Lin, Yajing; Yang, Chuangxin; Liang, Wanqi
刊名Chemical Engineering & Processing
2019
卷号Vol.135页码:68-81
关键词MESOPOROUS silica *MOLECULAR sieves *SILICA *IRON ions *OXIDATION-reduction reaction
ISSN号0255-2701
URL标识查看原文
公开日期[db:dc_date_available]
内容类型期刊论文
URI标识http://www.corc.org.cn/handle/1471x/4736621
专题湖南大学
作者单位1.Department of Ecology and Environmental Engineering, Guangdong Industry Technical College, Guangzhou, 510300, China
2.School of Eco-Environmental Engineering/Foshan research center for special functional building materials and its green preparation technology, Guangdong Industry Polytechnic, Guangzhou, 510300, China
推荐引用方式
GB/T 7714
Wan, Junjie,Feng, Xin,Li, Yu,et al. Effect of mesoporous silica molecular sieve coating on nZVI for 2,4-DCP degradation: Morphology and mechanism during the reaction.[J]. Chemical Engineering & Processing,2019,Vol.135:68-81.
APA Wan, Junjie.,Feng, Xin.,Li, Yu.,He, Jinqiang.,Zhao, Na.,...&Liang, Wanqi.(2019).Effect of mesoporous silica molecular sieve coating on nZVI for 2,4-DCP degradation: Morphology and mechanism during the reaction..Chemical Engineering & Processing,Vol.135,68-81.
MLA Wan, Junjie,et al."Effect of mesoporous silica molecular sieve coating on nZVI for 2,4-DCP degradation: Morphology and mechanism during the reaction.".Chemical Engineering & Processing Vol.135(2019):68-81.
个性服务
查看访问统计
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。


©版权所有 ©2017 CSpace - Powered by CSpace