CORC  > 金属研究所  > 中国科学院金属研究所
MECHANICAL-BEHAVIOR OF A CROSS-WEAVE CERAMIC MATRIX COMPOSITE .1. TENSILE AND COMPRESSIVE LOADING
Z. G. Wang ; C. Laird ; Z. Hashin ; B. W. Rosen ; C. F. Yen
刊名Journal of Materials Science
1991
卷号26期号:17页码:4751-4758
关键词fiber
ISSN号0022-2461
中文摘要The deformation and fracture processes of a cross-weave carbon fibre/SiC composite prepared by a chemical vapour deposition process has been explored by interrupted-loading tests and SEM examination of cracking and fracture processes. The tensile stress-strain curves show non-linear behaviour associated with progressive matrix cracking and spalling, and the occasional fracture of a fibre. Re-loading curves and compressive stress-strain curves show linear behaviour. The fracture process does not involve cracking by a single dominant crack but occurs by the development of multiple damage sites operating around the transverse fractures of groups of four to eight fibres followed by longitudinal cracking at their fibre-matrix interfaces and temporary arrest of the cracks, until specimen failure occurs and there is massive fibre debonding and pull-out.
原文出处://WOS:A1991GF00100027
公开日期2012-04-14
内容类型期刊论文
源URL[http://ir.imr.ac.cn/handle/321006/39471]  
专题金属研究所_中国科学院金属研究所
推荐引用方式
GB/T 7714
Z. G. Wang,C. Laird,Z. Hashin,et al. MECHANICAL-BEHAVIOR OF A CROSS-WEAVE CERAMIC MATRIX COMPOSITE .1. TENSILE AND COMPRESSIVE LOADING[J]. Journal of Materials Science,1991,26(17):4751-4758.
APA Z. G. Wang,C. Laird,Z. Hashin,B. W. Rosen,&C. F. Yen.(1991).MECHANICAL-BEHAVIOR OF A CROSS-WEAVE CERAMIC MATRIX COMPOSITE .1. TENSILE AND COMPRESSIVE LOADING.Journal of Materials Science,26(17),4751-4758.
MLA Z. G. Wang,et al."MECHANICAL-BEHAVIOR OF A CROSS-WEAVE CERAMIC MATRIX COMPOSITE .1. TENSILE AND COMPRESSIVE LOADING".Journal of Materials Science 26.17(1991):4751-4758.
个性服务
查看访问统计
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。


©版权所有 ©2017 CSpace - Powered by CSpace