Oxidation behavior of Al2O3 added reaction-sintered SiC ceramics in wet oxygen environment at 1300°C
Shan, Qingliang1,2,3,4; Hu, Jianbao1,2; Yang, Jinshan1,2; Kan, Yanmei1,2; Zhou, Haijun1,2; Zhu, Guangxiang1,2,4; Xue, Yudong1,2,4; Dong, Shaoming1,2
刊名Journal of Asian Ceramic Societies
2018
卷号6期号:3页码:254-261
DOI10.1080/21870764.2018.1504731
英文摘要The oxidation behavior of reaction-bonded SiC ceramics with Al2O3 was investigated at 1300°C for exposure duration up to 100 h under water vapor environment. Results show that Al2O3 is enriched on the oxidation surface, reducing the volatilization of the oxide layer and preventing the reduction of macroscopic size. Raman spectra results further testified that Al2O3 obviously improves the stability of glass structure and reduces the generation of non-bridged oxygen atoms (Si–O–H), which results in a lower reaction activity with steam of the aluminosilicate melt, therefore, significantly improving the oxidation resistance of SiC in O2/H2O atmosphere. ©, © 2018 The Author(s). Published by Informa UK Limited, trading as Taylor & Francis Group on behalf of The Korean Ceramic Society and The Ceramic Society of Japan.
出版者Taylor and Francis Ltd.
内容类型期刊论文
源URL[http://ir.sic.ac.cn/handle/331005/25189]  
专题中国科学院上海硅酸盐研究所
作者单位1.State Key Laboratory of High Performance Ceramics and Superne Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai, China;
2.Structural Ceramics and Composites Engineering Research Center, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai, China;
3.ShanghaiTech university, Shanghai, China;
4.University of Chinese Academy of Sciences, Beijing, China
推荐引用方式
GB/T 7714
Shan, Qingliang,Hu, Jianbao,Yang, Jinshan,et al. Oxidation behavior of Al2O3 added reaction-sintered SiC ceramics in wet oxygen environment at 1300°C[J]. Journal of Asian Ceramic Societies,2018,6(3):254-261.
APA Shan, Qingliang.,Hu, Jianbao.,Yang, Jinshan.,Kan, Yanmei.,Zhou, Haijun.,...&Dong, Shaoming.(2018).Oxidation behavior of Al2O3 added reaction-sintered SiC ceramics in wet oxygen environment at 1300°C.Journal of Asian Ceramic Societies,6(3),254-261.
MLA Shan, Qingliang,et al."Oxidation behavior of Al2O3 added reaction-sintered SiC ceramics in wet oxygen environment at 1300°C".Journal of Asian Ceramic Societies 6.3(2018):254-261.
个性服务
查看访问统计
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。


©版权所有 ©2017 CSpace - Powered by CSpace