中文摘要 | In this study cornstalk was used as reductant for reduction roasting of low-grade manganese dioxide ores, and sulfuric acid was used as leaching solvent for the roasted ore. The effects of weight ratio of ore to cornstalk, roasting temperature, roasting time, ore particle size, leaching temperature, stirring speed and sulfuric acid concentration on the leaching recovery were discussed. The leaching recovery of manganese reached 90.2% under the optimal condition which was determined as manganese dioxide ore to cornstalk weight ratio of 10:3, roasting temperature of 500 degrees C for 80 min, leaching stirring speed of 400 r/min. sulfuric acid concentration of 3 mol/L, leaching temperature of 50 degrees C for 40 min. (C) 2008 Elsevier B.V. All rights reserved. |
语种 | 英语 ; 英语 |
出版者 | ELSEVIER SCIENCE BV ; AMSTERDAM ; PO BOX 211, 1000 AE AMSTERDAM, NETHERLANDS |
内容类型 | 期刊论文 |
源URL | [http://hdl.handle.net/123456789/79276] |
专题 | 清华大学 |
推荐引用方式 GB/T 7714 | Cheng, Zhuo,Zhu, Guocai,Zhao, Yuna. Study in reduction-roast leaching manganese from low-grade manganese dioxide ores using cornstalk as reductant[J],2010, 2010. |
APA | Cheng, Zhuo,Zhu, Guocai,&Zhao, Yuna.(2010).Study in reduction-roast leaching manganese from low-grade manganese dioxide ores using cornstalk as reductant.. |
MLA | Cheng, Zhuo,et al."Study in reduction-roast leaching manganese from low-grade manganese dioxide ores using cornstalk as reductant".(2010). |
个性服务 |
查看访问统计 |
相关权益政策 |
暂无数据 |
收藏/分享 |
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。
修改评论